#106 |
The "Got Wood?" Thread
For metal, I sand any glossy finish out of the coating, then soak the part in hot water with TSP, available at Canadian Tire for like $3. Then clean off the smut that inevitably coats the item with a plastic scrubby, scrub brush, and dish detergent. Change the water and TSP often. It can take a while, even a day, but works for me every time.
Last edited by siggypoo; July 7th, 2014 at 18:14.. |
|
![]() |
![]() |
![]() |
#107 |
Don't like the APS wood stock original finishing even poor quality, sanded out the paint, hot burned graphics and re-stained and re-painted. Now it looks a lot better....
![]() ![]() ![]() ![]()
__________________
aka Uncle ![]() Last edited by N_Force; August 3rd, 2014 at 09:46.. |
|
![]() |
![]() |
![]() |
#108 |
That looks beautiful!
|
|
![]() |
![]() |
![]() |
#109 |
Well done. What did you use to seal the wood?
|
|
![]() |
![]() |
![]() |
#110 |
Thanks chaz your help and tips for the hot burning, much appreciated!
I sealed it with Minwax Fast-Drying Polyurethane (clear semi-gloss) in 2 layers.
__________________
aka Uncle ![]() Last edited by N_Force; August 3rd, 2014 at 16:23.. |
|
![]() |
![]() |
![]() |
#111 |
One of a shop in Hk got the full stock done for Hwashan double barrel. I'm going to plan for this project soon once I will have more free time!
![]()
__________________
aka Uncle ![]() Last edited by N_Force; October 14th, 2015 at 15:04.. |
|
![]() |
![]() |
![]() |
#112 |
dear airsofter fella
in near future ill start project to made a carving stock-lower body for BAR10/VSR10 sniper. advice please ![]() ![]() |
|
![]() |
![]() |
![]() |
#113 |
![]() ![]() ![]() On progress... carved woodkit for GHK/LCT AKM |
|
![]() |
![]() |
![]() |
#114 |
uploadfromtaptalk1446554569124.jpg
Ready to get rumble.... My carved woodkit for ghk/lct akm www.facebook.com/taringcarving |
|
![]() |
![]() |
![]() |
#115 |
Looks awesome!
|
|
![]() |
![]() |
![]() |
#116 |
![]() |
![]() |
![]() |
#117 |
Finally got this full size wood stock from octagon airsoft in Hong kong. Need a bit sand to make it a perfect fit, now looking for a right color stain to match the front hand grip.
![]() ![]()
__________________
aka Uncle ![]() Last edited by N_Force; November 7th, 2016 at 15:36.. |
|
![]() |
![]() |
![]() |
#118 |
Total rebuild and redo I did on an S&T Mosin Nagant. Sanded off that purple plastic shit, reshaped the stock and body, lowered stock arch by 1cm, removed brass caps, sanded to base wood, restained, aged.
Total time: 5ish days. ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]() ![]()
__________________
Peace through superior firepower. ![]() |
|
![]() |
![]() |
![]() |
#119 |
How did you do the lettering on the gun? Was it applied dry decal lettering or did you paint the letters then remove the paint from the surface leaving the paint in the recessed areas?
Excellent Nagant could pass for the real deal not an airsoft gun.... well done |
|
![]() |
![]() |
![]() |
#120 |
Can't Aim worth a damn!! old lady gives me heck for missing the toilet all the time.
|
Looks stunning, great workmanship!
|
![]() |
![]() |
![]() ![]() |
|
Bookmarks |
|
|
![]() |