Just a note:
*Tetrafluoroethane*
and
*Difluoromethane*
--
Input: I recall reading that Difluoromethane could potentially break down the seals and o-rings. You might want to read about this before continuing on using these, as I'm not sure at all about the validity of this statement.
As for myself, I use propane in my KWA M93R NS2. Aluminium slide, 32rounds mags.
Cooldown is noticeable but didn't impact performance much. At about 20 degrees Celsius, I could fire a good mag and a half, if not two, on full auto. That is with reloading the same mag after it's emptied.
Then again, the loading nozzle split in half after about 800-1000 rounds. I'm pretty sure it did becaise of a lack of lubrication between the nozzle and the slide's top, so it probably have nothing to do with the gas used. I hear KWA's pistols are meant to be used on greengas anyways, so...
Edit: yeah so I got beatten about the seals and difluoro :P that's what I get by typping on an iPhone :P
__________________
Quote:
Originally Posted by Brian McIlmoyle
Real life comparison,
GBBR- bang bang -- Giggle
AEG-- merrrzip merrzip -- meh
|
Last edited by MultipleParadox; May 15th, 2011 at 23:15..
|